Process guide · animated
Direct reduced iron and EAF steel: where to measure moisture, O₂ and CO₂
Follow the gas from natural gas desulfurisation through the reformer and shaft furnace to the seal gas and the electric arc furnace. Each numbered point shows what is measured, the typical value, why it matters and the analyzer that fits.
Tap a numbered point. Swipe the diagram sideways on a phone.
⤓ Download the 2-page PDF application note
How the process works
A natural-gas direct reduction plant turns iron ore pellets into DRI or HBI with a hot H₂/CO gas, and the electric arc furnace melts it into steel. Gas quality decides metallisation and energy use at every step. In the GCC, EMSTEEL runs HYL/Energiron-type modules, Hadeed and Jindal Shadeed (Sohar) run MIDREX-type modules, and the Duqm project uses a hydrogen-ready HYL/Energiron-type plant.
- Desulfurisation. Natural gas is cleaned to a narrow sulfur window: enough to stop carbon deposits in the reformer, not so much that the catalyst is poisoned.
- Reforming. Recycled top gas and natural gas are compressed, preheated and reformed over nickel catalyst. CO₂ and H₂O in the feed are the oxidants. HYL/Energiron-type plants reform inside the shaft instead.
- Reduction. Hot reducing gas, often boosted with oxygen injection, enters the shaft furnace at the bustle and reduces the iron ore.
- Top gas recycle. Spent top gas is scrubbed, cooled and split into recycle process gas and reformer fuel. HYL/Energiron-type plants remove CO₂ with amine.
- Seal gas and inerting. Dried flue gas or nitrogen seals the furnace and protects hot DRI and HBI from re-oxidation.
- Electric arc furnace. DRI or HBI is melted. Off-gas analysis controls post-combustion and detects water leaks.
Measurement points at a glance
| # | Point | Measures | Typical value / limit | Recommended solution |
|---|---|---|---|---|
| 1 | Natural gas at the plant battery limit | Water dew point at line pressure | Per the gas supply contract (no published limit for GCC plant supplies) | DPT990-EX |
| 2 | Desulfurised gas to the reformer | H₂S / total sulfur (ppmv) | Window of 2–5 ppmv in reformer feed (MIDREX-type). Raw associated gas has run 350–600 ppmv at one plant | Integrated system: ppm-level H₂S / total sulfur analyzer (GC with sulfur detector or UV) |
| 3 | Reformer feed gas (top gas + natural gas) | CO₂ (%) | About 15 % CO₂ (with ~13 % H₂O) in typical MIDREX-type feed gas | DPSS-61XX; Integrated system: NDIR CO₂ analyzer in a purged analyzer shelter |
| 4 | Reformer flue gas | Excess O₂ (%) | 1–2 % O₂; flue gas is roughly N₂ 60–65 %, CO₂ 15–18 %, H₂O 20–22 % | POA3500, DPSS-61XX, POA300, PGA530 |
| 5 | Reformed (bustle) gas | H₂, CO, CO₂, H₂O, CH₄ and quality ratio | Quality (H₂+CO)/(H₂O+CO₂) ≥ 9.5; typical H₂ 55 %, CO 35 % (MIDREX-type). HYL/Energiron-type gas runs H₂/CO 3–5 | Integrated system: process gas chromatograph or mass spectrometer |
| 6 | Bustle gas to the shaft furnace | CO₂ (%) | About 2 % in typical reformed gas; 2.8 % reported at one plant | DPSS-61XX; Integrated system: NDIR CO₂ analyzer with a low-percent range, in a purged analyzer shelter |
| 7 | Top gas leaving the furnace | H₂, CO, CO₂, CH₄ | Measured at one plant: H₂ 37 %, CO 19 %, CO₂ 14 %, H₂O 21 % | Integrated system: process gas chromatograph or mass spectrometer |
| 8 | Seal (inert) gas from reformer flue gas | O₂ (%) | Source flue gas below 2 % O₂; seal-gas specification set by the licensor | POA3500, POA300, PGA530, PGA500-EX |
| 9 | Dry seal gas after the dryer | Dew point | Set by the licensor's seal-gas specification | DPT810, DPT830 |
| 10 | Nitrogen header for inerting (HYL/Energiron-type) | O₂ and dew point | N₂ use of about 12 (cold DRI) to 19 Nm³/t (HBI); purity per plant specification | PGA500, POA200, DPT830 |
| 11 | EAF off-gas after the elbow | CO, CO₂, O₂, H₂ (H₂O for water leaks) | One control scheme keeps the CO/O₂ ratio between 0.40 and 0.75 | Integrated system: water-cooled extractive probe with NDIR / paramagnetic / thermal-conductivity analyzers, or in-situ laser (TDLAS) |
| 12 | Oxygen for bustle-gas injection and EAF lancing | O₂ purity (%) | > 99.5 % from cryogenic air separation; < 95 % from VPSA | POA3500 |
Values are typical figures from published specifications and technical literature. Your contract, licensor or plant specification always governs.
Getting reliable readings
- Dry basis. Reformer and bustle gases carry several percent water. Condition the sample and report CO₂ and O₂ on a dry basis, or use a fully heated line.
- Hot, dusty, flammable gas. Top gas, bustle gas and EAF off-gas need cooled or blow-back probes, fast loops and certified analyzer cabinets.
- Seal gas is a safety loop. Its O₂ and dew point decide whether hot DRI re-oxidises and whether the seal legs stay non-flammable.
- Many points are integrated systems. Gas chromatographs, sulfur analyzers and EAF off-gas systems are supplied as integrated systems together with YORK dew point, O₂ and CO₂ instruments.
References
- ENERGIRON technology: DRI-EAF production route using natural gas or H₂European Commission, Innovation Centre for Industrial Transformation
- Quatravaux et al., Adaptation of the Rist operating diagram for the direct reduction shaft, Metals 11 (2021) 1953MDPI
- MIDREX ProcessKobelco Technology Review No. 29
- Krassnig et al., EAF post-combustion control by on-line laser-based off-gas measurementArchives of Metallurgy and Materials 53(2), 2008
- Risonarta et al., Optimization of the EAF process at Deutsche EdelstahlwerkeArchives of Metallurgy and Materials 53(2), 2008
- Hurskainen, Industrial oxygen demand in Finland (VTT-R-06563-17)VTT
- Carriage of DRI (risk alert)Steamship Mutual
- Emsteel Abu Dhabi steel plantGlobal Energy Monitor
- Pilot scale direct reduction with hydrogenHYBRIT
- Midrex provides SULB operational flexibility (feed-gas sulfur window)Midrex
Related
Frequently asked questions
Which gas measurements matter most in a DRI plant?
Sulfur in the reformer feed, CO₂ and H₂O in the feed and reducing gas, reformer flue gas O₂, and the O₂ and dew point of the seal or inert gas that protects hot DRI.
What is the bustle gas quality ratio?
It is (H₂+CO)/(H₂O+CO₂), the reducing gases divided by the oxidising gases. MIDREX-type plants keep it at 9.5 or higher.
Why measure the seal gas?
Seal gas keeps reducing gas in the furnace and air out. Too much oxygen or moisture re-oxidises hot DRI and can create a flammable mixture at the seal legs.
Can YORK supply the gas chromatographs and EAF off-gas systems?
YORK supplies them as integrated systems through its partner integration factory, together with YORK dew point, oxygen and CO₂ analyzers.
Planning analyzers for a DRI or EAF plant?
Send us the measurement points, gas conditions and area classification, and we will propose instruments and sampling systems.